HomeCompany InformationProductsCustomer ServiceNewsroomInvestor Relations

DLC Film (Anti-wear Application)

Better Performance for You

1. Applications:
KINIK company offers DLC coating for Anti-wear applicatio by PECVD (Plasma Enhance Chemical Vapor Deposition ).KINIK Company has good experience of DLC coating on CD mold, Plunger, Golf driver, Automotive engine parts,injetion Molds,Sliding parts,Glass,and pluger..etc.
 
2. KINIK’s experience in the DLC coatings:
 

Transparent DLC for Passivation Layer

Visible transmittance:   Tave. @400~700 nm = 88%

 
3. Overall characteristics of KINIK DLC coatings:
The thickness of DLC film varies normally from 1 to 3 um.
Coating type Microhardness HV (Measurement by Vickers) Coefficient of friction (against steel, dry conditions) Roughness Maximum working temperature (℃) Deposition temperature (℃)
Normal DLC 3500~5000 0.05~0.1.5 Conformal Coating 350 < 200
Ultra low friction DLC 3500~4000 <0.05 Conformal Coating 400 < 200
 
For comparison:
TiN 2000 0.4 Ra: 0.15 um
RTM: 0.5 um
550 400~450
TiAlN 2800 0.4 Ra: 0.2 um
RTM: 2.0 um
800 400~450
TiCN 3000 0.3 Ra: 0.2 um
RTM: 2.0 um
450 400~500
CrN 1850 0.45 Ra: 0.15 um
RTM: 2.0 um
700 200~300
 
Customer Service:kevin@kinik.com.tw